不锈钢, 17, 7PH,箔, FeCr17Ni7, Annealed-Condition A Temper, 0.075mm厚
材料 >> 合金
品牌: Goodfellow产地: 英国
留言咨询
产品介绍
| 订货号 | 包装规格 |
| Disc |
| 765-318-11 | 4mm |
| 664-772-91 | 6mm |
| 096-613-50 | 8mm |
| 076-689-39 | 10mm |
| 586-169-16 | 15mm |
| 271-146-67 | 25mm |
| 893-327-80 | 50mm |
| Coil |
| 290-030-82 | 300mm x 0.5m |
| 952-368-92 | 300mm x 1m |
| 046-122-50 | 300mm x 2m |
| Sizes |
| 174-057-82 | 25mm x 25mm |
| 757-227-55 | 50mm x 50mm |
| 653-446-19 | 100mm x 100mm |
| 680-764-90 | 150mm x 150mm |
| 095-618-98 | 300mm x 300mm |
产品参数
| Coil Width[卷材宽度] | 300mm |
| Diameter[直径] | 4mm - 50mm |
| Grade[等级] | Precipitation Hardenable |
| Temper[状态] | Annealed - Condition A |
| Thickness[厚度] | 0.075mm |
| Typical Analysis(典型分析) |
| Al | 1.15 Percent |
| C | 700 PPM |
| Cr | 17 Percent |
| Mn | 7000 PPM |
| Ni | 7 Percent |
| Si | 4000 PPM |
| Thermal Properties(热性能) |
| Coefficient of thermal expansion ( x10⁻⁶ K⁻¹ ) | 15.300 @20-90℃ |
| Melting point ( C ) | 1435.00 |
| Thermal conductivity ( W m⁻¹ K⁻¹ ) | 16.70 @23℃ |
| Mechanical Properties(机械性能) |
| Elongation at break ( % ) | < 25.0 |
| Izod impact strength ( J m⁻¹ ) | 61.0 - - 115.0 |
| Modulus of elasticity ( GPa ) | 214.0 |
| Tensile strength ( MPa ) | 1020.00 - 1550.00 |
| Physical Properties(物理性质) |
| Density ( g cm⁻³ ) | 7.810 |
| Electrical Properties(电气特性) |
| Electrical resistivity ( μOhmcm ) | 80-85 |
其他参数
公差
| 长度 | <100mm | ±1mm |
|---|
| ≥100mm | +2% / -1% |
| 直径 | <100mm | ±1mm |
|---|
| ≥100mm | +2% / -1% |
| 厚度 | <0.01mm | ±25% |
|---|
| ≤0.05mm | ±15% |
| >0.05mm | ±10% |
| 长度 1 | <100mm | ±1mm |
|---|
| ≥100mm | +2% / -1% |
| 长度 2 | <100mm | ±1mm |
|---|
| ≥100mm | +2% / -1% |