| Temper[状态] | As Rolled |
| Thickness[厚度] | 5mm |
| Typical Analysis(典型分析) |
| Al | 5 Percent |
| C | 0.02 Percent |
| Cr | 22 Percent |
| Mn | 0.2 Percent |
| Si | 0.3 Percent |
| Y | 0.1 Percent |
| Zr | 0.1 Percent |
| Thermal Properties(热性能) |
| Coefficient of thermal expansion ( x10⁻⁶ K⁻¹ ) | 11.100 @20-100℃ |
| Maximum use temperature in air ( C ) | 1100 - 1300 |
| Melting point ( C ) | 1380.00 - 1490.00 |
| Thermal conductivity ( W m⁻¹ K⁻¹ ) | 16.00 @23℃ |
| Magnetic(磁性) |
| Curie temperature ( C ) | 600 |
| Mechanical Properties(机械性能) |
| Elongation at break ( % ) | < 25.0 |
| Hardness - Vickers ( kgf mm⁻² ) | 230 |
| Tensile strength ( MPa ) | 560.00 |
| Electrical Properties(电气特性) |
| Electrical resistivity ( μOhmcm ) | 134 |
| Temperature coefficient ( K⁻¹ ) | 0.00010 |
| Physical Properties(物理性质) |
| Density ( g cm⁻³ ) | 7.220 |